Differential Scanning Calorimetry Performance Comparison
18 Jan 2012
Differential scanning calorimetry (DSC) is a commonly used technique for studying polymeric, pharmaceutical, and energetic materials. This note compares various instruments data when performing routine measurements on a standard polystyrene (PS) and low density polyethylene (PE) sample using the conventional heat-cool-reheat method.